General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 370 [-] Show Supplier Material materials with Dureza Brinell of 370 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 0 % Show Supplier Material materials with Elongación of 0 % | in 2″ (51 mm) |
Límite elástico | 23.0 °C | 476 MPa Show Supplier Material materials with Límite elástico of 476 MPa | |
Resistencia a la tracción | 23.0 °C | 558 MPa Show Supplier Material materials with Resistencia a la tracción of 558 MPa |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminio | 14 - 15 % Show Supplier Material materials with Aluminio of 14 - 15 % | ||
Cobre | Balance, including silver | ||
Hierro | 3 - 5 % Show Supplier Material materials with Hierro of 3 - 5 % | ||
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 0.04 % Show Supplier Material materials with Silicona of 0.04 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Draw dies, Wear shoes, Wear strips, Slides, Forming dies, Wear plates, Cams, Welding AMPCO® 25 |