General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 364 [-] Show Supplier Material materials with Dureza Brinell of 364 [-] | (3000 kg), Three layer deposit on mild steel |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Fabrication of new rebuilding of worn, ferrous dies, used for forming or drawing titanium, stainless steel, low to medium carbon steel | |
Other | AMPCO-CORE® 300 is available from stock in two diameters: 0.045” (1.2mm) and 0,062” (1.6mm). Both sizes are available in 12″ (300mm) spools weighing 33lb (15 kg) each. Other diameters are available upon request. | |
Processing methods | Welding position and deposits: The flat welding position is recommended. Backhand (trailing) welding is preferred rather than forehand (pushing) to make either stringer or weaved beads. Shielding gas: 100% Argon |