General
Property | Value |
---|---|
Recycled Content | 80 % Show Supplier Material materials with Recycled Content of 80 % |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Dureza Brinell | 23.0 °C | 54 [-] Show Supplier Material materials with Dureza Brinell of 54 [-] | BHN (3000kg) 1/4″ (6.4mm) deposit |
Elongación | 23.0 °C | 29 % Show Supplier Material materials with Elongación of 29 % | in 2″ (51 mm) |
Estricción | 23.0 °C | 45 % Show Supplier Material materials with Estricción of 45 % | |
Límite elástico | 23.0 °C | 55 MPa Show Supplier Material materials with Límite elástico of 55 MPa | |
Resistencia a la tracción | 23.0 °C | 200 MPa Show Supplier Material materials with Resistencia a la tracción of 200 MPa |
Eléctrico
Property | Value |
---|---|
Specific Electrical conductivity | 40 % IACS Show Supplier Material materials with Specific Electrical conductivity of 40 % IACS |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Cobre | Balance, including silver | ||
Estaño | 1 % Show Supplier Material materials with Estaño of 1 % | max. | |
Fósforo | 0.15 % Show Supplier Material materials with Fósforo of 0.15 % | max. | |
Manganeso | 0.5 % Show Supplier Material materials with Manganeso of 0.5 % | max. | |
Otro | 0.5 % Show Supplier Material materials with Otro of 0.5 % | max. | |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Welding: Billet molds, Conductor rolls, Heater elements, Copper sculptures, Steel mill electrode holders, Bus bars, Copper connectors |