General
Property | Value | Comment | |
---|---|---|---|
Carbon equivalent (CEV) | 0.43 [-] Show Supplier Material materials with Carbon equivalent (CEV) of 0.43 [-] | Cast | |
Carbon equivalent note | CEV = C + Mn/6 + (Cr+Mo+V)/5 + (Cu+Ni)/15 and PCM = C + Si/30 + (Cr+Mn+Cu)/20 + Ni/60 + Mo/15 + V/10 + 5B |
Mecánica
Property | Temperature | Value | Comment |
---|---|---|---|
Elongación | 22 % Show Supplier Material materials with Elongación of 22 % | min. A5.65√So | for thickness 5-40 mm | Transverse | |
Energía de impacto Charpy | -40 °C | 50 J Show Supplier Material materials with Energía de impacto Charpy of 50 J | min. | for thickness 5-40 mm |
Límite elástico | 345 MPa Show Supplier Material materials with Límite elástico of 345 MPa | min. | for thickness 16-40 mm | Transverse | |
355 MPa Show Supplier Material materials with Límite elástico of 355 MPa | min. | for thickness 5-16 mm | Transverse | ||
Resistencia a la tracción | 470 - 610 MPa Show Supplier Material materials with Resistencia a la tracción of 470 - 610 MPa | for thickness 5-40 mm | Transverse |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminio | 0.02 % Show Supplier Material materials with Aluminio of 0.02 % | min. | for thickness 5-40 mm |
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. | for thickness 5-40 mm |
Carbono | 0.14 % Show Supplier Material materials with Carbono of 0.14 % | max. | for thickness 5-40 mm |
Fósforo | 0.03 % Show Supplier Material materials with Fósforo of 0.03 % | max. | for thickness 5-40 mm |
Manganeso | 1.6 % Show Supplier Material materials with Manganeso of 1.6 % | max. | for thickness 5-40 mm |
Molibdeno | 0.2 % Show Supplier Material materials with Molibdeno of 0.2 % | max. | for thickness 5-40 mm |
Niobio | 0.05 % Show Supplier Material materials with Niobio of 0.05 % | max. | for thickness 5-40 mm |
Nitrógeno | 0.015 % Show Supplier Material materials with Nitrógeno of 0.015 % | max. | for thickness 5-40 mm |
Níquel | 0.3 % Show Supplier Material materials with Níquel of 0.3 % | max. | for thickness 5-40 mm |
Silicona | 0.5 % Show Supplier Material materials with Silicona of 0.5 % | max. | for thickness 5-40 mm |
Titanio | 0.05 % Show Supplier Material materials with Titanio of 0.05 % | max. | for thickness 5-40 mm |
Vanadio | 0.1 % Show Supplier Material materials with Vanadio of 0.1 % | max. | for thickness 5-40 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore structures such as platforms and equipment for new offshore windmill towers. | |
Chemical composition | The above chemical properties are based on cast analysis data. Product analysis may be requested at the time of order. | |
Delivery condtion | For the dimensions available please visit Dimension tables (see Table A). Table A with a thickness range as indicated in the Mechanical properties. | |
Other | Available options Options available (after previous agreement): |