Unclassified Low Alloy Steel
EN 10025-4 Grade S275M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S275ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S355M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S355ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S420M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S420ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10025-4 Grade S460ML thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420M thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML1 thermomechanically rolledSuministrada por:
2 proveedores de Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P355M thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P355ML1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P355ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P420ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460M thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460ML1 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Unclassified Low Alloy Steel
EN 10028-5 Grade P460ML2 thermomechanically rolledSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A829 Grade 4142 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaSuministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
ASTM A829 Grade 4140 As-Rolled, Annealed, Normalized, Normalized and Tempered, or Quenched and Tempered; Tensile strength range 100 MPaSuministrada por:
1 proveedor Matmatch
Unclassified Stainless Steel
ASTM A543 Class 1 Type B Quenched and TemperedSuministrada por:
1 proveedor Matmatch