Kepstan® 7002

Nombres alternativos y comerciales
PEKK
Want to keep this datasheet? Save it now in your required format

Description

KEPSTAN® PEKK resin is a high performance thermoplastic material, based on PolyEtherKetoneKetone (PEKK) highly stable chemical backbone. Its semi crystalline structure in solid state offers an outstanding combination of mechanical and thermal strength together with chemical and fire resistance.

Among the KEPSTAN® family, the 7000 Series benefits uniquely from PEKK crystalline capabilities while reducing significantly processing temperatures compared to the more crystalline 8000 Series. With a reduced melting temperature (® decreased by 25°C) and a Tg above 160°C, the KEPSTAN® 7000 Series resins are highly enabling in the field of continuous fiber composites for structural applications.

KEPSTAN® 7000 Series includes a medium flow grade, KEPSTAN® 7002, and a high flow grade, KEPSTAN® 7003, both unfilled PEKK resins designed to meet the requirements of a broad range of melt processing technologies, including among others extrusion, injection molding, fiber impregnation, consolidation and composite forming technologies.

KEPSTAN® PEKK resin is available in pellet form and in powder form with different particle sizes. Standard packaging includes 20 kg boxes for pellets and 10 kg boxes for powders.

Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.

A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Propiedades

General

PropertyValueConditionTesting Standard

Densidad

1.29 g/cm³

Show Supplier Material materials with Densidad of 1.29 g/cm³

dry

ISO 1183

Índice límite de óxigeno

35 %

Show Supplier Material materials with Índice límite de óxigeno of 35 %

dry

ISO 4589-1/-2

Mecánica

PropertyTemperatureValueConditionTesting Standard

Módulo elástico

3.8 GPa

Show Supplier Material materials with Módulo elástico of 3.8 GPa

dry

ISO 527-1/-2

Resistencia al choque, ensayo Charpy entallado

-30 °C

4.5 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m²

dry

ISO 179/1eA

23 °C

4.5 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 4.5 kJ/m²

dry

ISO 179/1eA

Resistencia al choque, ensayo Charpy no entallado

-30 °C

41 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 41 kJ/m²

dry

ISO 179/1eU

23 °C

62 kJ/m²

Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 62 kJ/m²

dry

ISO 179/1eU

Aplicaciones térmicas

PropertyValueConditionTesting StandardPressure

Temperatura de flexión bajo carga

172 °C

Show Supplier Material materials with Temperatura de flexión bajo carga of 172 °C

dry

ISO 75-1/-2

2 MPa

Eléctrico

PropertyValueConditionFrequencyTesting Standard

Constante dieléctrica

2.6 [-]

Show Supplier Material materials with Constante dieléctrica of 2.6 [-]

dry

1MHz

IEC 60250

Rheological Properties

PropertyValueConditionTesting StandardComment

Velocidad de flujo del volumen derretido

6 cm³/10min

Show Supplier Material materials with Velocidad de flujo del volumen derretido of 6 cm³/10min

dry

ISO 1133

380°C/1kg

Technological properties

Property
Processing methods

Injection Molding:

  • Drying temperature and time: 150°C for 3 to 4 hours or 120°C for 6 to 8 hours
  • Processing temperature: 340 – 360°C
  • Temperature settings - Injection: Rear 320°C / Center 340°C / Front 350°C / Nozzle 360°C
  • Mold temperature (to facilitate filling of the cavity and polymer crystallization): 230 - 250°C
  • Temperature settings - Extrusion Zones 1/2/3/4: 290°C/ 320°C/ 350°C/ 340°C Die: 340°C