General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.29 g/cm³ Show Supplier Material materials with Densidad of 1.29 g/cm³ | dry | ISO 1183 |
Índice límite de óxigeno | 35 % Show Supplier Material materials with Índice límite de óxigeno of 35 % | dry | ISO 4589-1/-2 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Módulo elástico | 3.8 GPa Show Supplier Material materials with Módulo elástico of 3.8 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | dry | ISO 179/1eU | No Break at 23°C |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure |
---|---|---|---|---|
Temperatura de flexión bajo carga | 175 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 175 °C | dry | ISO 75-1/-2 | 2 MPa |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Constante dieléctrica | 2.6 [-] Show Supplier Material materials with Constante dieléctrica of 2.6 [-] | dry | 1MHz | IEC 60250 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | dry | ISO 1133 | 380°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Metal Tube Coating,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Monofilaments,Connectors E&E,Performance Wire,Wire and Cables,Natural Gas Distribution- Fittings,Natural Gas Distribution- Pipes,Offshore Flexible Pipes | |
Processing methods | Injection Molding: |