General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.45 g/cm³ Show Supplier Material materials with Densidad of 1.45 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | dry | ISO 179/1eA |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 34 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 34 kJ/m² | dry | ISO 179/1eU |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 18 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 18 cm³/10min | dry | ISO 1133 | 380°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fittings, Components, and Injection Molded Parts,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes | |
Fillers | 40% Carbon Fiber | |
Processing methods | Injection Molding: |