General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.62 g/cm³ Show Supplier Material materials with Densidad of 1.62 g/cm³ | dry | ISO 1183 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 5 cm³/10min | dry | ISO 1133 | 380°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Connectors,Fittings, Components, and Injection Molded Parts,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Connectors E&E | |
Fillers | 40% Glass Fiber | |
Processing methods | Injection Molding: |