Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Kynar 500® FSF® PVDF resin is used by leading coating formulators as a base vehicle in long-life coatings for aluminum, galvanized steel and aluminized steel.
Today,
Kynar 500® FSF® PVDF resin-based metal coatings provide billions of square feet of protection against weathering, aging and pollution on commercial, industrial, institutional and residential buildings around the globe. The capability of Kynar 500® resins to deliver long-term durability is unparalleled in the industry. Introduced in 1965, Kynar 500® resin-based coatings were the original high performance finishes for architectural metal. According to a recent survey, Kynar 500® finishes are still the architect’s first choice.
Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.
All categories
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Límite elástico | 21 MPa Show Supplier Material materials with Límite elástico of 21 MPa | dry | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Application areas | Factory Applied |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.