Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Kynar Aquatec®
is an innovative platform of emulsions, which are used by paint formulators to make premium weatherable water-based coatings.
Coatings formulated with these emulsions can provide the durability and performance of traditional Kynar 500® based coatings. They can easily be applied to a variety of substrates, including metals, plastics, wood, concrete, textiles, and previously painted surfaces. Now, the extreme weatherability of a
Kynar 500®
based coating is available in a VOC-compliant, field or factory applied, ambient air-dry system. Additional benefits include tremendous resistance to dirt pick-up, outstanding water repellency, and high initial and long-term Total Solar Reflectance and Emissivity.
Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.
All categories
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Límite elástico | 21 MPa Show Supplier Material materials with Límite elástico of 21 MPa | dry | ISO 527-1/-2 |
Technological properties
Property | ||
---|---|---|
Application areas | Factory Applied,Field Applied |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.