General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
0.03 - 0.06 % Show Supplier Material materials with Absorción de agua of 0.03 - 0.06 % | ASTM D570 | |||
Coefficient of friction | 0.54 [-] Show Supplier Material materials with Coefficient of friction of 0.54 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.55 [-] Show Supplier Material materials with Coefficient of friction of 0.55 [-] | ASTM D1894 | vs Steel, Static | ||
Densidad | 1.78 - 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.78 - 1.8 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry | ||
Índice límite de óxigeno | 43 % Show Supplier Material materials with Índice límite de óxigeno of 43 % | ASTM D2863 | ||
49 % Show Supplier Material materials with Índice límite de óxigeno of 49 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 57 - 62 [-] Show Supplier Material materials with Dureza Shore D of 57 - 62 [-] | ASTM D2240 | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal |
200 - 400 % Show Supplier Material materials with Elongación of 200 - 400 % | ASTM D638 | |||
Elongation at yield | 15 - 25 % Show Supplier Material materials with Elongation at yield of 15 - 25 % | ASTM D638 | ||
15 % Show Supplier Material materials with Elongation at yield of 15 % | ISO 527-1/-2 | dry | ||
Límite elástico | 13.8 - 21.4 MPa Show Supplier Material materials with Límite elástico of 13.8 - 21.4 MPa | ASTM D638 | ||
27 MPa Show Supplier Material materials with Límite elástico of 27 MPa | ISO 527-1/-2 | dry | ||
Módulo de flexión | 0.276 - 0.414 GPa Show Supplier Material materials with Módulo de flexión of 0.276 - 0.414 GPa | ASTM D790 | ||
Módulo elástico | 0.276 - 0.448 GPa Show Supplier Material materials with Módulo elástico of 0.276 - 0.448 GPa | ASTM D638 | ||
0.526 GPa Show Supplier Material materials with Módulo elástico of 0.526 GPa | ISO 527-1/-2 | dry | ||
Resistencia a la compresión | 24.1 - 31 MPa Show Supplier Material materials with Resistencia a la compresión of 24.1 - 31 MPa | ASTM D695 | ||
Resistencia a la flexión | 13.8 - 24.1 MPa Show Supplier Material materials with Resistencia a la flexión of 13.8 - 24.1 MPa | ASTM D790 | at 5% strain | |
Resistencia a la tracción | 20 - 27.6 MPa Show Supplier Material materials with Resistencia a la tracción of 20 - 27.6 MPa | ASTM D638 | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | ISO 179/1eA | dry |
Aplicaciones térmicas
Property | Value | Testing Standard | Condition | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000162 - 0.000216 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000162 - 0.000216 1/K | ASTM D696 | |||||||
0.000177 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000177 1/K | ISO 11359-1/-2 | dry | |||||||
Conductividad térmica | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Temperatura de flexión bajo carga | 35 - 52 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 35 - 52 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
43 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 43 °C | ISO 75-1/-2 | dry | 2 MPa | ||||||
49 - 66 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 49 - 66 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
57 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 57 °C | ISO 75-1/-2 | dry | 0.45 MPa | ||||||
Temperatura de fusión | 130 - 138 °C Show Supplier Material materials with Temperatura de fusión of 130 - 138 °C | ASTM D3418 | |||||||
134 °C Show Supplier Material materials with Temperatura de fusión of 134 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de reblandecimiento Vicat | 61 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 61 °C | ISO 306 | 50°C/h 50N | ||||||
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ASTM D7028, ISO 11357-1/-2 | dry | 10°C/min | |||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Eléctrico
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Constante dieléctrica | 3.8 - 12.1 [-] Show Supplier Material materials with Constante dieléctrica of 3.8 - 12.1 [-] | 1KHz | ASTM D150 | |
7 [-] Show Supplier Material materials with Constante dieléctrica of 7 [-] | 1MHz | IEC 60250 | dry | |
11.5 [-] Show Supplier Material materials with Constante dieléctrica of 11.5 [-] | 100Hz | IEC 60250 | dry | |
Factor de disipación | 0.02 - 0.24 [-] Show Supplier Material materials with Factor de disipación of 0.02 - 0.24 [-] | 100KHz | ASTM D150 | |
0.024 [-] Show Supplier Material materials with Factor de disipación of 0.024 [-] | 100Hz | IEC 60250 | dry | |
Rigidez dieléctrica | 43.3 - 51.2 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 43.3 - 51.2 kV/mm | ASTM D149 | ||
Surface resistivity | 4.8e+11 - 5.1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 4.8e+11 - 5.1e+11 Ω/sq | ASTM D257 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de refracción | 1 [-] Show Supplier Material materials with Índice de refracción of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 2000 - 2500 Pa·s Show Supplier Material materials with Melt viscosity of 2000 - 2500 Pa·s | ASTM D3835 | ||
Velocidad de flujo de la masa derretida | 4 - 14 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4 - 14 g/10min | ASTM D1238 | 230°C/12.5kg | |
Velocidad de flujo del volumen derretido | 1.9 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 1.9 cm³/10min | ISO 1133 | dry | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines,Chemical Process Industry,Tubing and Hoses,Performance Wire,Offshore Umbilicals | |
Processing methods | Injection Molding: |