General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.77 - 1.8 g/cm³ | ASTM D792 |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 70 - 75 [-] Show Supplier Material materials with Dureza Shore D of 70 - 75 [-] | ASTM D2240 | ||
Elongación | 30 - 200 % Show Supplier Material materials with Elongación of 30 - 200 % | ASTM D638 | ||
Límite elástico | 31 - 41.4 MPa Show Supplier Material materials with Límite elástico of 31 - 41.4 MPa | ASTM D638 | ||
40 MPa Show Supplier Material materials with Límite elástico of 40 MPa | ISO 527-1/-2 | dry | ||
Módulo de flexión | 1.0 - 1.2 GPa Show Supplier Material materials with Módulo de flexión of 1.0 - 1.2 GPa | ASTM D790 | ||
Resistencia a la compresión | 41.4 - 58.6 MPa Show Supplier Material materials with Resistencia a la compresión of 41.4 - 58.6 MPa | ASTM D695 | ||
Resistencia a la flexión | 20.7 - 34.5 MPa Show Supplier Material materials with Resistencia a la flexión of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | |
Resistencia a la tracción | 27.6 - 48.3 MPa Show Supplier Material materials with Resistencia a la tracción of 27.6 - 48.3 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Testing Standard |
---|---|---|
Temperatura de fusión | 155 - 160 °C Show Supplier Material materials with Temperatura de fusión of 155 - 160 °C | ASTM D3418 |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | 65% RH | ASTM D257 |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 2300 - 2700 Pa·s Show Supplier Material materials with Melt viscosity of 2300 - 2700 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Plenum Pipe,Wire and Cables |