General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
Coefficient of friction | 0.19 [-] Show Supplier Material materials with Coefficient of friction of 0.19 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.26 [-] Show Supplier Material materials with Coefficient of friction of 0.26 [-] | ASTM D1894 | vs Steel, Static | ||
Densidad | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.77 - 1.8 g/cm³ | ASTM D792 | ||
1.77 g/cm³ Show Supplier Material materials with Densidad of 1.77 g/cm³ | ISO 1183 | dry | ||
Índice límite de óxigeno | 43 % Show Supplier Material materials with Índice límite de óxigeno of 43 % | ASTM D2863 |
Mecánica
Property | Temperature | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Dureza Shore D | 70 - 75 [-] Show Supplier Material materials with Dureza Shore D of 70 - 75 [-] | ASTM D2240 | |||
Elongación | 30 - 200 % Show Supplier Material materials with Elongación of 30 - 200 % | ASTM D638 | |||
50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal | ||
Elongation at yield | 5 - 15 % Show Supplier Material materials with Elongation at yield of 5 - 15 % | ASTM D638 | |||
11 % Show Supplier Material materials with Elongation at yield of 11 % | ISO 527-1/-2 | dry | |||
Impact strength, Charpy notched, ASTM | 23 °C | 160 - 427 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 160 - 427 J/m | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | |||
Límite elástico | 17 MPa Show Supplier Material materials with Límite elástico of 17 MPa | ISO 527-1/-2 | dry | ||
31 - 41.4 MPa Show Supplier Material materials with Límite elástico of 31 - 41.4 MPa | ASTM D638 | ||||
Módulo de flexión | 1.0 - 1.2 GPa Show Supplier Material materials with Módulo de flexión of 1.0 - 1.2 GPa | ASTM D790 | |||
Módulo elástico | 1.0 - 1.5 GPa Show Supplier Material materials with Módulo elástico of 1.0 - 1.5 GPa | ASTM D638 | |||
1.3 GPa Show Supplier Material materials with Módulo elástico of 1.3 GPa | ISO 527-1/-2 | dry | |||
Resistencia a la compresión | 41.4 - 58.6 MPa Show Supplier Material materials with Resistencia a la compresión of 41.4 - 58.6 MPa | ASTM D695 | |||
Resistencia a la flexión | 20.7 - 34.5 MPa Show Supplier Material materials with Resistencia a la flexión of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | ||
Resistencia a la tracción | 27.6 - 48.3 MPa Show Supplier Material materials with Resistencia a la tracción of 27.6 - 48.3 MPa | ASTM D638 | |||
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | ISO 179/1eA | dry |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Condition | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000126 - 0.000185 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000126 - 0.000185 1/K | ASTM D696 | |||||||
Conductividad térmica | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | UL 746B | |||||||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | UL 746B | |||||||
Temperatura de flexión bajo carga | 38 - 55 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 38 - 55 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
60 - 75 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 - 75 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Temperatura de fusión | 155 - 160 °C Show Supplier Material materials with Temperatura de fusión of 155 - 160 °C | ASTM D3418 | |||||||
157 °C Show Supplier Material materials with Temperatura de fusión of 157 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de transición del vidrio | -40.6 - -38.3 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40.6 - -38.3 °C | ASTM D7028 | |||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available |
Eléctrico
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Constante dieléctrica | 3.5 - 10.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.5 - 10.2 [-] | 1KHz | ASTM D150 | |
6.85 [-] Show Supplier Material materials with Constante dieléctrica of 6.85 [-] | 100Hz | IEC 60250 | dry | |
Factor de disipación | 1.2e-05 [-] Show Supplier Material materials with Factor de disipación of 1.2e-05 [-] | 100Hz | IEC 60250 | dry |
0.01 - 0.22 [-] Show Supplier Material materials with Factor de disipación of 0.01 - 0.22 [-] | 100KHz | ASTM D150 | ||
Rigidez dieléctrica | 1.4 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 1.4 kV/mm | IEC 60243-1 | dry | |
51.2 - 63 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 51.2 - 63 kV/mm | ASTM D149 | |||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH | |
2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de refracción | 1 [-] Show Supplier Material materials with Índice de refracción of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt viscosity | 1600 - 2000 Pa·s Show Supplier Material materials with Melt viscosity of 1600 - 2000 Pa·s | ASTM D3835 | |
Velocidad de flujo de la masa derretida | 9 - 16 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 9 - 16 g/10min | ASTM D1238 | 230°C/12.5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Chemical Process Industry - Injection Molding,Foamed PVDF Cable Jacketing,Performance Wire,Underground Fuel Containment |