Kynar Flex® 2950-05

Nombres alternativos y comerciales
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® 2950-05 resin is a pelletized, semi-crystalline VF2 based copolymer. It has been designed for wire and cable applications requiring high flexibility and improved resistance to impact.The low molecular weight allows extrusion conditions that reduce jacket shrink back over fiber optic constructions.

Additional characteristics:

  • Excellent thermal stability
  • Excellent abrasion resistance
  • Excellent chemical resistance
  • Impervious to UV degradation
  • High Limiting Oxygen Index
  • Extremely low smoke emission characteristics

    Meets UL910 requirements

  • Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.

    A menos que se indique lo contrario, todas las medidas corresponden a condiciones de temperatura ambiente. A menos que se indique lo contrario, se utilizan las unidades del SI.
    Las normas armonizadas son similares a uno o varios estándares del proveedor. Es posible que algunas normas armonizadas se ajusten al estándar original, mientras que otras pueden quedar fuera de su alcance.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Propiedades

    General

    PropertyValueTesting StandardConditionComment

    Absorción de agua

    0.03 %

    Show Supplier Material materials with Absorción de agua of 0.03 %

    Sim. to ISO 62

    0.03 - 0.05 %

    Show Supplier Material materials with Absorción de agua of 0.03 - 0.05 %

    ASTM D570

    Coefficient of friction

    0.54 [-]

    Show Supplier Material materials with Coefficient of friction of 0.54 [-]

    ASTM D1894

    vs Steel, Kinetic

    0.55 [-]

    Show Supplier Material materials with Coefficient of friction of 0.55 [-]

    ASTM D1894

    vs Steel, Static

    Densidad

    1.77 - 1.8 g/cm³

    Show Supplier Material materials with Densidad of 1.77 - 1.8 g/cm³

    ASTM D792

    1.77 g/cm³

    Show Supplier Material materials with Densidad of 1.77 g/cm³

    ISO 1183

    dry

    Índice límite de óxigeno

    95 %

    Show Supplier Material materials with Índice límite de óxigeno of 95 %

    ASTM D2863, ISO 4589-1/-2

    dry

    Mecánica

    PropertyValueTesting StandardConditionComment

    Dureza Shore D

    57 - 62 [-]

    Show Supplier Material materials with Dureza Shore D of 57 - 62 [-]

    ASTM D2240

    Elongación

    50 %

    Show Supplier Material materials with Elongación of 50 %

    ISO 527-1/-2

    dry

    min. | nominal

    200 - 400 %

    Show Supplier Material materials with Elongación of 200 - 400 %

    ASTM D638

    Elongation at yield

    15 - 25 %

    Show Supplier Material materials with Elongation at yield of 15 - 25 %

    ASTM D638

    18 %

    Show Supplier Material materials with Elongation at yield of 18 %

    ISO 527-1/-2

    dry

    Impact strength, Charpy notched, ASTM

    No Break at 23°C

    ASTM D256

    Impact strength, Charpy unnotched, ASTM

    No Break at 23°C

    ASTM D256

    Límite elástico

    12 MPa

    Show Supplier Material materials with Límite elástico of 12 MPa

    ISO 527-1/-2

    dry

    13.8 - 21.4 MPa

    Show Supplier Material materials with Límite elástico of 13.8 - 21.4 MPa

    ASTM D638

    Módulo de flexión

    0.276 - 0.414 GPa

    Show Supplier Material materials with Módulo de flexión of 0.276 - 0.414 GPa

    ASTM D790

    Módulo elástico

    0.276 - 0.448 GPa

    Show Supplier Material materials with Módulo elástico of 0.276 - 0.448 GPa

    ASTM D638

    0.387 GPa

    Show Supplier Material materials with Módulo elástico of 0.387 GPa

    ISO 527-1/-2

    dry

    Resistencia a la compresión

    24.1 - 31 MPa

    Show Supplier Material materials with Resistencia a la compresión of 24.1 - 31 MPa

    ASTM D695

    Resistencia a la flexión

    13.8 - 24.1 MPa

    Show Supplier Material materials with Resistencia a la flexión of 13.8 - 24.1 MPa

    ASTM D790

    at 5% strain

    Resistencia a la tracción

    20 - 27.6 MPa

    Show Supplier Material materials with Resistencia a la tracción of 20 - 27.6 MPa

    ASTM D638

    Resistencia al choque, ensayo Charpy entallado

    No Break at 23°C

    ISO 179/1eA

    dry

    Aplicaciones térmicas

    PropertyValueTesting StandardPressureConditionComment

    Calor específico

    745 - 958 J/(kg·K)

    Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K)

    DSC

    Coeficiente de dilatación térmica

    0.000162 - 0.000216 1/K

    Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000162 - 0.000216 1/K

    ASTM D696

    Conductividad térmica

    0.144 - 0.18 W/(m·K)

    Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K)

    ASTM D433

    Temperatura de flexión bajo carga

    35 - 52 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 35 - 52 °C

    ASTM D648

    2 MPa

    248 °F/hr

    43 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 43 °C

    ISO 75-1/-2

    2 MPa

    dry

    49 - 66 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 49 - 66 °C

    ASTM D648

    0.45 MPa

    248 °F/hr

    57 °C

    Show Supplier Material materials with Temperatura de flexión bajo carga of 57 °C

    ISO 75-1/-2

    0.45 MPa

    dry

    Temperatura de fusión

    130 - 138 °C

    Show Supplier Material materials with Temperatura de fusión of 130 - 138 °C

    ASTM D3418

    134 °C

    Show Supplier Material materials with Temperatura de fusión of 134 °C

    ISO 11357-1/-3

    dry

    10°C/min

    Temperatura de transición del vidrio

    -42.2 - -40 °C

    Show Supplier Material materials with Temperatura de transición del vidrio of -42.2 - -40 °C

    ASTM D7028

    -40 °C

    Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C

    ISO 11357-1/-2

    dry

    10°C/min

    Thermal decomposition in air

    375 °C

    Show Supplier Material materials with Thermal decomposition in air of 375 °C

    TGA

    1% wt. loss

    Thermal decomposition in nitrogen

    410 °C

    Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

    TGA

    1% wt. loss

    Inflamabilidad

    At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available

    Eléctrico

    PropertyValueFrequencyTesting StandardCondition

    Constante dieléctrica

    3.8 - 12.1 [-]

    Show Supplier Material materials with Constante dieléctrica of 3.8 - 12.1 [-]

    1KHz

    ASTM D150

    7.05 [-]

    Show Supplier Material materials with Constante dieléctrica of 7.05 [-]

    100Hz

    IEC 60250

    dry

    Factor de disipación

    1.2e-05 [-]

    Show Supplier Material materials with Factor de disipación of 1.2e-05 [-]

    100Hz

    IEC 60250

    dry

    0.02 - 0.24 [-]

    Show Supplier Material materials with Factor de disipación of 0.02 - 0.24 [-]

    100KHz

    ASTM D150

    Rigidez dieléctrica

    1.4 kV/mm

    Show Supplier Material materials with Rigidez dieléctrica of 1.4 kV/mm

    IEC 60243-1

    dry

    43.3 - 51.2 kV/mm

    Show Supplier Material materials with Rigidez dieléctrica of 43.3 - 51.2 kV/mm

    ASTM D149

    Volume resistivity

    2e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

    ASTM D257

    65% RH

    2e+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm

    IEC 60093

    dry

    Rheological Properties

    PropertyValueTesting StandardConditionComment

    Melt viscosity

    6 - 1200 Pa·s

    Show Supplier Material materials with Melt viscosity of 6 - 1200 Pa·s

    ASTM D3835

    Velocidad de flujo de la masa derretida

    8 - 25 g/10min

    Show Supplier Material materials with Velocidad de flujo de la masa derretida of 8 - 25 g/10min

    ASTM D1238

    230°C/3.8kg

    Velocidad de flujo del volumen derretido

    11.5 cm³/10min

    Show Supplier Material materials with Velocidad de flujo del volumen derretido of 11.5 cm³/10min

    ISO 1133

    dry

    232°C/3.8kg

    Technological properties

    Property
    Application areas

    Automotive Cables,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables