General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Absorción de agua | 0.5 % Show Supplier Material materials with Absorción de agua of 0.5 % | ASTM D570 | max. |
Densidad | 1.78 - 1.82 g/cm³ Show Supplier Material materials with Densidad of 1.78 - 1.82 g/cm³ | ASTM D792 | |
Índice límite de óxigeno | 43 % Show Supplier Material materials with Índice límite de óxigeno of 43 % | ASTM D2863 |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 50 - 60 [-] Show Supplier Material materials with Dureza Shore D of 50 - 60 [-] | ASTM D2240 | ||
Elongación | 500 % Show Supplier Material materials with Elongación of 500 % | ASTM D638 | min. | |
Elongation at yield | 25 - 40 % Show Supplier Material materials with Elongation at yield of 25 - 40 % | ASTM D638 | ||
Impact strength, Charpy notched, ASTM | No Break at 23°C | ASTM D256 | ||
Límite elástico | 11.7 - 15.9 MPa Show Supplier Material materials with Límite elástico of 11.7 - 15.9 MPa | ASTM D638 | ||
27 MPa Show Supplier Material materials with Límite elástico of 27 MPa | ISO 527-1/-2 | dry | ||
Módulo de flexión | 0.248 - 0.303 GPa Show Supplier Material materials with Módulo de flexión of 0.248 - 0.303 GPa | ASTM D790 | ||
Módulo elástico | 0.207 - 0.345 GPa Show Supplier Material materials with Módulo elástico of 0.207 - 0.345 GPa | ASTM D638 | ||
Resistencia a la tracción | 18.6 - 24.1 MPa Show Supplier Material materials with Resistencia a la tracción of 18.6 - 24.1 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Testing Standard |
---|---|---|
Coeficiente de dilatación térmica | 0.000153 - 0.000194 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000153 - 0.000194 1/K | ASTM D696 |
Temperatura de fusión | 160 - 168 °C Show Supplier Material materials with Temperatura de fusión of 160 - 168 °C | ASTM D3418 |
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ASTM D7028 |
Eléctrico
Property | Value | Testing Standard | Condition |
---|---|---|---|
Rigidez dieléctrica | 39.4 - 47.2 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 39.4 - 47.2 kV/mm | ASTM D149 | |
Surface resistivity | 7.6e+11 - 7.9e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 7.6e+11 - 7.9e+11 Ω/sq | ASTM D257 | |
Volume resistivity | 7.8e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 7.8e+13 Ω·cm | ||
8e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 8e+13 Ω·cm | ASTM D257 | 65% RH |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt viscosity | 2100 - 2600 Pa·s Show Supplier Material materials with Melt viscosity of 2100 - 2600 Pa·s | ASTM D3835 | |
Velocidad de flujo de la masa derretida | 2.5 - 7.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 2.5 - 7.5 g/10min | ASTM D1238 | 230°C/12.5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Auto - Water Cooling Circuit,Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables |