General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 - 0.05 % Show Supplier Material materials with Absorción de agua of 0.03 - 0.05 % | ASTM D570 | ||
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.31 [-] Show Supplier Material materials with Coefficient of friction of 0.31 [-] | ASTM D1894 | vs Steel, Static | ||
Densidad | 1.77 - 1.8 g/cm³ Show Supplier Material materials with Densidad of 1.77 - 1.8 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry | ||
Índice límite de óxigeno | 95 % Show Supplier Material materials with Índice límite de óxigeno of 95 % | ASTM D2863, ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 65 - 70 [-] Show Supplier Material materials with Dureza Shore D of 65 - 70 [-] | ASTM D2240 | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal |
300 - 500 % Show Supplier Material materials with Elongación of 300 - 500 % | ASTM D638 | |||
Elongation at yield | 10 - 20 % Show Supplier Material materials with Elongation at yield of 10 - 20 % | ASTM D638 | ||
15 % Show Supplier Material materials with Elongation at yield of 15 % | ISO 527-1/-2 | dry | ||
Impact strength, Charpy notched, ASTM | No Break at 23°C | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | ||
Límite elástico | 24.1 - 34.5 MPa Show Supplier Material materials with Límite elástico of 24.1 - 34.5 MPa | ASTM D638 | ||
27 MPa Show Supplier Material materials with Límite elástico of 27 MPa | ISO 527-1/-2 | dry | ||
Módulo de flexión | 0.621 - 0.827 GPa Show Supplier Material materials with Módulo de flexión of 0.621 - 0.827 GPa | ASTM D790 | ||
Módulo elástico | 0.689 - 1.2 GPa Show Supplier Material materials with Módulo elástico of 0.689 - 1.2 GPa | ASTM D638 | ||
0.7 GPa Show Supplier Material materials with Módulo elástico of 0.7 GPa | ISO 527-1/-2 | dry | ||
Resistencia a la compresión | 31 - 41.4 MPa Show Supplier Material materials with Resistencia a la compresión of 31 - 41.4 MPa | ASTM D695 | ||
Resistencia a la flexión | 20.7 - 34.5 MPa Show Supplier Material materials with Resistencia a la flexión of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | |
Resistencia a la tracción | 34.5 - 48.3 MPa Show Supplier Material materials with Resistencia a la tracción of 34.5 - 48.3 MPa | ASTM D638 | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | ISO 179/1eA | dry |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Condition | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000126 - 0.000185 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000126 - 0.000185 1/K | ASTM D696 | |||||||
Conductividad térmica | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | UL 746B | |||||||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746B | |||||||
Temperatura de flexión bajo carga | 43 - 54 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 43 - 54 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
48 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 48 °C | ISO 75-1/-2 | 2 MPa | dry | ||||||
54 - 77 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 54 - 77 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
65 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 65 °C | ISO 75-1/-2 | 0.45 MPa | dry | ||||||
Temperatura de fusión | 161 - 168 °C Show Supplier Material materials with Temperatura de fusión of 161 - 168 °C | ASTM D3418 | |||||||
164 °C Show Supplier Material materials with Temperatura de fusión of 164 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de transición del vidrio | -41.1 - -39.4 °C Show Supplier Material materials with Temperatura de transición del vidrio of -41.1 - -39.4 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 IEC 60695-11-10: V-0 and yellow card available |
Eléctrico
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Constante dieléctrica | 3.2 - 10.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 - 10.2 [-] | 1KHz | ASTM D150 | |
6.7 [-] Show Supplier Material materials with Constante dieléctrica of 6.7 [-] | 100Hz | IEC 60250 | dry | |
Factor de disipación | 1.05e-05 [-] Show Supplier Material materials with Factor de disipación of 1.05e-05 [-] | 100Hz | IEC 60250 | dry |
0.02 - 0.19 [-] Show Supplier Material materials with Factor de disipación of 0.02 - 0.19 [-] | 100KHz | ASTM D150 | ||
Rigidez dieléctrica | 51.2 - 59.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 51.2 - 59.1 kV/mm | ASTM D149 | ||
Surface resistivity | 5.9e+11 - 6.1e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5.9e+11 - 6.1e+11 Ω/sq | ASTM D257 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | IEC 60093 | dry |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 600 - 1200 Pa·s Show Supplier Material materials with Melt viscosity of 600 - 1200 Pa·s | ASTM D3835 | ||
Velocidad de flujo de la masa derretida | 4 - 18 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 4 - 18 g/10min | ASTM D1238 | 230°C/3.8kg | |
Velocidad de flujo del volumen derretido | 4 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 4 cm³/10min | ISO 1133 | dry | 232°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables | |
Processing methods | Compression Molding: |