General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
0.03 - 0.05 % Show Supplier Material materials with Absorción de agua of 0.03 - 0.05 % | ASTM D570 | |||
Coefficient of friction | 0.3 [-] Show Supplier Material materials with Coefficient of friction of 0.3 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.31 [-] Show Supplier Material materials with Coefficient of friction of 0.31 [-] | ASTM D1894 | vs Steel, Static | ||
Densidad | 1.75 - 1.77 g/cm³ Show Supplier Material materials with Densidad of 1.75 - 1.77 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry | ||
Índice límite de óxigeno | 42 % Show Supplier Material materials with Índice límite de óxigeno of 42 % | ASTM D2863 | ||
43 % Show Supplier Material materials with Índice límite de óxigeno of 43 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 65 - 70 [-] Show Supplier Material materials with Dureza Shore D of 65 - 70 [-] | ASTM D2240 | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal |
300 - 500 % Show Supplier Material materials with Elongación of 300 - 500 % | ASTM D638 | |||
Elongation at yield | 10 - 20 % Show Supplier Material materials with Elongation at yield of 10 - 20 % | ASTM D638 | ||
15 % Show Supplier Material materials with Elongation at yield of 15 % | ISO 527-1/-2 | dry | ||
Impact strength, Charpy notched, ASTM | No Break at 23°C | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | ||
Límite elástico | 12 MPa Show Supplier Material materials with Límite elástico of 12 MPa | ISO 527-1/-2 | dry | |
24.1 - 34.5 MPa Show Supplier Material materials with Límite elástico of 24.1 - 34.5 MPa | ASTM D638 | |||
Módulo de flexión | 0.621 - 0.827 GPa Show Supplier Material materials with Módulo de flexión of 0.621 - 0.827 GPa | ASTM D790 | ||
Módulo elástico | 0.689 - 1.2 GPa Show Supplier Material materials with Módulo elástico of 0.689 - 1.2 GPa | ASTM D638 | ||
0.7 GPa Show Supplier Material materials with Módulo elástico of 0.7 GPa | ISO 527-1/-2 | dry | ||
Resistencia a la compresión | 34.5 - 48.3 MPa Show Supplier Material materials with Resistencia a la compresión of 34.5 - 48.3 MPa | ASTM D695 | ||
Resistencia a la flexión | 20.7 - 34.5 MPa Show Supplier Material materials with Resistencia a la flexión of 20.7 - 34.5 MPa | ASTM D790 | at 5% strain | |
Resistencia a la tracción | 34.5 - 48.3 MPa Show Supplier Material materials with Resistencia a la tracción of 34.5 - 48.3 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Condition | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000126 - 0.000185 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000126 - 0.000185 1/K | ASTM D696 | |||||||
Conductividad térmica | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | UL 746B | |||||||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746B | |||||||
Temperatura de flexión bajo carga | 43 - 54 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 43 - 54 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
50 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 50 °C | ISO 75-1/-2 | 2 MPa | dry | ||||||
54 - 77 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 54 - 77 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Temperatura de fusión | 161 - 168 °C Show Supplier Material materials with Temperatura de fusión of 161 - 168 °C | ASTM D3418 | |||||||
165 °C Show Supplier Material materials with Temperatura de fusión of 165 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de transición del vidrio | -41.1 - -39.4 °C Show Supplier Material materials with Temperatura de transición del vidrio of -41.1 - -39.4 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 IEC 60695-11-10: V-0 and yellow card available, 5V at thickness 1 mm IEC 60695-11-20: 5VA |
Eléctrico
Property | Value | Frequency | Testing Standard |
---|---|---|---|
Constante dieléctrica | 3.2 - 10.2 [-] Show Supplier Material materials with Constante dieléctrica of 3.2 - 10.2 [-] | 1KHz | ASTM D150 |
Factor de disipación | 0.02 - 0.19 [-] Show Supplier Material materials with Factor de disipación of 0.02 - 0.19 [-] | 100KHz | ASTM D150 |
Rigidez dieléctrica | 51.2 - 59.1 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 51.2 - 59.1 kV/mm | ASTM D149 | |
Surface resistivity | 5.3e+11 - 5.5e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 5.3e+11 - 5.5e+11 Ω/sq | ASTM D257 |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de refracción | 1 [-] Show Supplier Material materials with Índice de refracción of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 2000 - 2600 Pa·s Show Supplier Material materials with Melt viscosity of 2000 - 2600 Pa·s | ASTM D3835 | ||
Velocidad de flujo de la masa derretida | 2.5 - 7.5 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 2.5 - 7.5 g/10min | ASTM D1238 | 230°C/12.5kg | |
Velocidad de flujo del volumen derretido | 0.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 0.5 cm³/10min | ISO 1133 | dry | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids,Photovoltaic / Solar Film | |
Processing methods | Compression Molding: |