General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
Densidad | 1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183, ASTM D792 | dry | min. |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | min. | nominal |
400 % Show Supplier Material materials with Elongación of 400 % | ASTM D638 | min. | ||
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
Límite elástico | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | ASTM D638 | ||
Módulo de flexión | 1.0 GPa Show Supplier Material materials with Módulo de flexión of 1.0 GPa | ASTM D790 | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Temperatura de fusión | 151 - 157 °C Show Supplier Material materials with Temperatura de fusión of 151 - 157 °C | ASTM D3418 | ||
154 °C Show Supplier Material materials with Temperatura de fusión of 154 °C | ISO 11357-1/-3 | dry | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 3400 - 3800 Pa·s Show Supplier Material materials with Melt viscosity of 3400 - 3800 Pa·s | ASTM D3835 | ||
Velocidad de flujo de la masa derretida | 3 - 8 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 3 - 8 g/10min | ASTM D1238 | 230°C/21.6kg | |
Velocidad de flujo del volumen derretido | 3.2 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3.2 cm³/10min | ISO 1133 | dry | 232°C/21.6kg |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder,Lithium ion Battery Separator Coating |