Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
Materiales
Categories
No estás conectado
Categories
Encontrar proveedores de metales
List Your Company
Case Studies
Tools
Sobre nosotros
Kynar Flex® PPA 2200
Kynar Flex® resins are fluorinated thermoplastic copolymers.
Kynar Flex® PPA 2200 resin is specially designed pellet used as a polymer process aid (PPA) for polyolefins. The use of Kynar Flex® PPA 2200 resin at 200-1000 ppm levels reduces extruder pressure, improves surface finish, reduces die build up, and improves gauge control.
Los datos sobre este material han sido proporcionados por Arkema Technical Polymers.
All categories
General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 0.7 g/cm³ Show Supplier Material materials with Densidad of 0.7 g/cm³ | dry | ISO 1183 |
Densidad aparente | 0.6 - 0.8 g/cm³ Show Supplier Material materials with Densidad aparente of 0.6 - 0.8 g/cm³ |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 144 °C Show Supplier Material materials with Temperatura de fusión of 144 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
EMPRESA
CONTÁCTANOS
Siebenbürger Str. 23, 86983 Lechbruck am See, Germany
© 2024 Plansee Composite Materials GmbH, All rights reserved.