General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 0.7 g/cm³ Show Supplier Material materials with Densidad of 0.7 g/cm³ | dry | ISO 1183 |
Densidad aparente | 0.5 - 0.9 g/cm³ Show Supplier Material materials with Densidad aparente of 0.5 - 0.9 g/cm³ |
Mecánica
Property | Value | Condition | Testing Standard |
---|---|---|---|
Límite elástico | 15 MPa Show Supplier Material materials with Límite elástico of 15 MPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 165 °C Show Supplier Material materials with Temperatura de fusión of 165 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | dry | ISO 11357-1/-2 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluoropolymer Processing Aids |