General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
0.04 % Show Supplier Material materials with Absorción de agua of 0.04 % | ASTM D570 | max. | ||
Densidad | 1.77 g/cm³ Show Supplier Material materials with Densidad of 1.77 g/cm³ | ISO 1183 | dry | |
1.8 - 1.83 g/cm³ Show Supplier Material materials with Densidad of 1.8 - 1.83 g/cm³ | ASTM D792 | |||
Índice límite de óxigeno | 40 % Show Supplier Material materials with Índice límite de óxigeno of 40 % | ASTM D2863, ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 35 - 43 [-] Show Supplier Material materials with Dureza Shore D of 35 - 43 [-] | ASTM D2240 | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal |
500 % Show Supplier Material materials with Elongación of 500 % | ASTM D638 | min. | ||
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | ISO 527-1/-2 | dry | |
25 - 35 % Show Supplier Material materials with Elongation at yield of 25 - 35 % | ASTM D638 | |||
Límite elástico | 4.8 - 8.3 MPa Show Supplier Material materials with Límite elástico of 4.8 - 8.3 MPa | ASTM D638 | ||
Módulo de flexión | 0.0689 - 0.138 GPa Show Supplier Material materials with Módulo de flexión of 0.0689 - 0.138 GPa | ASTM D790 | ||
Módulo elástico | 0.0345 - 0.103 GPa Show Supplier Material materials with Módulo elástico of 0.0345 - 0.103 GPa | ASTM D638 | ||
0.08 GPa Show Supplier Material materials with Módulo elástico of 0.08 GPa | ISO 527-1/-2 | dry | ||
Resistencia a la tracción | 9.0 - 20.7 MPa Show Supplier Material materials with Resistencia a la tracción of 9.0 - 20.7 MPa | ASTM D638 | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | ISO 179/1eA | dry |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Temperatura de flexión bajo carga | 46 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 46 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 92 - 112 °C Show Supplier Material materials with Temperatura de fusión of 92 - 112 °C | ASTM D3418 | |||
101 °C Show Supplier Material materials with Temperatura de fusión of 101 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ASTM D7028 |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 1200 - 2000 Pa·s Show Supplier Material materials with Melt viscosity of 1200 - 2000 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Tubing and Hoses |