General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.03 % Show Supplier Material materials with Absorción de agua of 0.03 % | Sim. to ISO 62 | ||
0.07 % Show Supplier Material materials with Absorción de agua of 0.07 % | ASTM D570 | max. | ||
Coefficient of friction | 0.49 [-] Show Supplier Material materials with Coefficient of friction of 0.49 [-] | ASTM D1894 | vs Steel, Static | |
0.54 [-] Show Supplier Material materials with Coefficient of friction of 0.54 [-] | ASTM D1894 | vs Steel, Kinetic | ||
Densidad | 1.79 g/cm³ Show Supplier Material materials with Densidad of 1.79 g/cm³ | ISO 1183 | dry | |
1.8 - 1.82 g/cm³ Show Supplier Material materials with Densidad of 1.8 - 1.82 g/cm³ | ASTM D792 | |||
Índice límite de óxigeno | 42 % Show Supplier Material materials with Índice límite de óxigeno of 42 % | ASTM D2863 | ||
44 % Show Supplier Material materials with Índice límite de óxigeno of 44 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore D | 50 - 57 [-] Show Supplier Material materials with Dureza Shore D of 50 - 57 [-] | ASTM D2240 | ||
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal |
500 - 800 % Show Supplier Material materials with Elongación of 500 - 800 % | ASTM D638 | |||
Elongation at yield | 17 - 25 % Show Supplier Material materials with Elongation at yield of 17 - 25 % | ASTM D638 | ||
18 % Show Supplier Material materials with Elongation at yield of 18 % | ISO 527-1/-2 | dry | ||
Impact strength, Charpy notched, ASTM | No Break at 23°C | ASTM D256 | ||
Impact strength, Charpy unnotched, ASTM | No Break at 23°C | ASTM D256 | ||
Límite elástico | 11.7 - 19.3 MPa Show Supplier Material materials with Límite elástico of 11.7 - 19.3 MPa | ASTM D638 | ||
15 MPa Show Supplier Material materials with Límite elástico of 15 MPa | ISO 527-1/-2 | dry | ||
Módulo de flexión | 0.193 - 0.276 GPa Show Supplier Material materials with Módulo de flexión of 0.193 - 0.276 GPa | ASTM D790 | ||
Módulo elástico | 0.241 - 0.379 GPa Show Supplier Material materials with Módulo elástico of 0.241 - 0.379 GPa | ASTM D638 | ||
0.35 GPa Show Supplier Material materials with Módulo elástico of 0.35 GPa | ISO 527-1/-2 | dry | ||
Resistencia a la compresión | 13.8 - 20.7 MPa Show Supplier Material materials with Resistencia a la compresión of 13.8 - 20.7 MPa | ASTM D695 | ||
Resistencia a la flexión | 10.3 - 17.2 MPa Show Supplier Material materials with Resistencia a la flexión of 10.3 - 17.2 MPa | ASTM D790 | at 5% strain | |
Resistencia a la tracción | 13.8 - 31 MPa Show Supplier Material materials with Resistencia a la tracción of 13.8 - 31 MPa | ASTM D638 | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | ISO 179/1eA | dry |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Condition | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000153 - 0.000194 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000153 - 0.000194 1/K | ASTM D696 | |||||||
Conductividad térmica | 0.144 - 0.18 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.144 - 0.18 W/(m·K) | ASTM D433 | |||||||
Temperatura de flexión bajo carga | 27 - 38 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 27 - 38 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
31 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 31 °C | ISO 75-1/-2 | 2 MPa | dry | ||||||
Temperatura de fusión | 117 - 125 °C Show Supplier Material materials with Temperatura de fusión of 117 - 125 °C | ASTM D3418 | |||||||
122 °C Show Supplier Material materials with Temperatura de fusión of 122 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de transición del vidrio | -43.3 - -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -43.3 - -40 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 mm IEC 60695-11-10: V-0 and yellow card available |
Eléctrico
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Constante dieléctrica | 4.5 - 13.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 - 13.5 [-] | 1KHz | ASTM D150 | |
Factor de disipación | 0.05 - 0.29 [-] Show Supplier Material materials with Factor de disipación of 0.05 - 0.29 [-] | 100KHz | ASTM D150 | |
Rigidez dieléctrica | 12 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 12 kV/mm | IEC 60243-1 | dry | |
31.5 - 43.3 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 31.5 - 43.3 kV/mm | ASTM D149 | |||
Surface resistivity | 8.5e+11 - 9.2e+11 Ω/sq Show Supplier Material materials with Surface resistivity of 8.5e+11 - 9.2e+11 Ω/sq | ASTM D257 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de refracción | 1 [-] Show Supplier Material materials with Índice de refracción of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 900 - 1600 Pa·s Show Supplier Material materials with Melt viscosity of 900 - 1600 Pa·s | ASTM D3835 | ||
Velocidad de flujo de la masa derretida | 1 - 15 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 1 - 15 g/10min | ASTM D1238 | 230°C/3.8kg | |
Velocidad de flujo del volumen derretido | 5.8 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 5.8 cm³/10min | ISO 1133 | dry | 232°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Chemical Process Industry - Injection Molding,Fluoropolymer Processing Aids,Tubing and Hoses,Automotive Cables,Performance Wire,Plenum Cable,Lithium Ion Battery Binder | |
Certifications | Yellow Card |