General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.73 g/cm³ Show Supplier Material materials with Densidad of 1.73 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 40 % Show Supplier Material materials with Elongación of 40 % | dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 15 % Show Supplier Material materials with Elongation at yield of 15 % | dry | ISO 527-1/-2 | ||
Módulo elástico | 1 GPa Show Supplier Material materials with Módulo elástico of 1 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 10.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 10.6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 51 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 51 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.000183 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000183 1/K | dry | ISO 11359-1/-2 | ||
Temperatura de flexión bajo carga | 67 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 67 °C | dry | ISO 75-1/-2 | 2 MPa | |
Temperatura de fusión | 171 °C Show Supplier Material materials with Temperatura de fusión of 171 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Specific heat capacity melt | 1600 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1600 J/(kg·K) | |||
Thermal conductivity of melt | 0.19 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K) | |||
Velocidad de flujo del volumen derretido | 3 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3 cm³/10min | dry | ISO 1133 | 230°C/10kg |
Technological properties
Property | ||
---|---|---|
Application areas | Offshore Flexible Pipes | |
Processing methods | Injection Molding: |