General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 0.02 % Show Supplier Material materials with Absorción de agua of 0.02 % | Sim. to ISO 62 | |
Densidad | 1.77 g/cm³ Show Supplier Material materials with Densidad of 1.77 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.015 % Show Supplier Material materials with Moisture absorption of 0.015 % | Sim. to ISO 62 | |
Índice límite de óxigeno | 80 % Show Supplier Material materials with Índice límite de óxigeno of 80 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 40 % Show Supplier Material materials with Elongación of 40 % | dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | dry | ISO 527-1/-2 | ||
Límite elástico | 54 MPa Show Supplier Material materials with Límite elástico of 54 MPa | dry | ISO 527-1/-2 | ||
Módulo elástico | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 5 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 12 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | -30 °C | 221 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 221 kJ/m² | dry | ISO 179/1eU | |
23 °C | 227 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 227 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00015 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00015 1/K | dry | ISO 11359-1/-2 | ||||||
Temperatura de flexión bajo carga | 108 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 108 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Temperatura de fusión | 171 °C Show Supplier Material materials with Temperatura de fusión of 171 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Temperatura de reblandecimiento Vicat | 140 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 140 °C | ISO 306 | 50°C/h 50N | ||||||
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Constante dieléctrica | 7 [-] Show Supplier Material materials with Constante dieléctrica of 7 [-] | dry | 1MHz | IEC 60250 |
9.5 [-] Show Supplier Material materials with Constante dieléctrica of 9.5 [-] | dry | 100Hz | IEC 60250 | |
Factor de disipación | 0.028 [-] Show Supplier Material materials with Factor de disipación of 0.028 [-] | dry | 100Hz | IEC 60250 |
0.22 [-] Show Supplier Material materials with Factor de disipación of 0.22 [-] | dry | 1MHz | IEC 60250 | |
Rigidez dieléctrica | 24 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 24 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1.5e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1.5e+14 Ω/sq | cond. | IEC 60093 | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | dry | IEC 60093 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 2 % Show Supplier Material materials with Contracción of 2 % | dry | ISO 294-4 | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | ISO 294-4 | Transverse | |
Velocidad de flujo del volumen derretido | 6.7 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 6.7 cm³/10min | dry | ISO 1133 | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes | |
Processing methods | Injection Molding: |