General
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Absorción de agua | 0.02 % Show Supplier Material materials with Absorción de agua of 0.02 % | Sim. to ISO 62 | ||
0.05 % Show Supplier Material materials with Absorción de agua of 0.05 % | ASTM D570 | max. | ||
Coefficient of friction | 0.14 [-] Show Supplier Material materials with Coefficient of friction of 0.14 [-] | ASTM D1894 | vs Steel, Kinetic | |
0.2 [-] Show Supplier Material materials with Coefficient of friction of 0.2 [-] | ASTM D1894 | vs Steel, Static | ||
Densidad | 1.77 - 1.79 g/cm³ Show Supplier Material materials with Densidad of 1.77 - 1.79 g/cm³ | ASTM D792 | ||
1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry | ||
Índice límite de óxigeno | 42 % Show Supplier Material materials with Índice límite de óxigeno of 42 % | ASTM D2863 | ||
43 % Show Supplier Material materials with Índice límite de óxigeno of 43 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Temperature | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|---|
Dureza Shore D | 76 - 80 [-] Show Supplier Material materials with Dureza Shore D of 76 - 80 [-] | ASTM D2240 | |||
Elongación | 10 - 50 % Show Supplier Material materials with Elongación of 10 - 50 % | ASTM D638 | |||
50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | dry | min. | nominal | ||
Elongation at yield | 5 - 10 % Show Supplier Material materials with Elongation at yield of 5 - 10 % | ASTM D638 | |||
8 % Show Supplier Material materials with Elongation at yield of 8 % | ISO 527-1/-2 | dry | |||
Impact strength, Charpy notched, ASTM | 53.4 - 107 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 53.4 - 107 J/m | ASTM D256 | |||
Límite elástico | 44.8 - 55.2 MPa Show Supplier Material materials with Límite elástico of 44.8 - 55.2 MPa | ASTM D638 | |||
54 MPa Show Supplier Material materials with Límite elástico of 54 MPa | ISO 527-1/-2 | dry | |||
Módulo de flexión | 1.4 - 2.3 GPa Show Supplier Material materials with Módulo de flexión of 1.4 - 2.3 GPa | ASTM D790 | |||
Módulo elástico | 1.4 - 2.3 GPa Show Supplier Material materials with Módulo elástico of 1.4 - 2.3 GPa | ASTM D638 | |||
2.4 GPa Show Supplier Material materials with Módulo elástico of 2.4 GPa | ISO 527-1/-2 | dry | |||
Resistencia a la compresión | 68.9 - 103 MPa Show Supplier Material materials with Resistencia a la compresión of 68.9 - 103 MPa | ASTM D695 | |||
Resistencia a la flexión | 58.6 - 75.8 MPa Show Supplier Material materials with Resistencia a la flexión of 58.6 - 75.8 MPa | ASTM D790 | at 5% strain | ||
Resistencia a la tracción | 34.5 - 55.2 MPa Show Supplier Material materials with Resistencia a la tracción of 34.5 - 55.2 MPa | ASTM D638 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 6 kJ/m² | ISO 179/1eA | dry | |
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 50 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 50 kJ/m² | ISO 179/1eU | dry |
Aplicaciones térmicas
Property | Value | Testing Standard | Pressure | Condition | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Calor específico | 745 - 958 J/(kg·K) Show Supplier Material materials with Calor específico of 745 - 958 J/(kg·K) | DSC | |||||||
Coeficiente de dilatación térmica | 0.000119 - 0.000144 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000119 - 0.000144 1/K | ASTM D696 | |||||||
Conductividad térmica | 0.17 - 0.19 W/(m·K) Show Supplier Material materials with Conductividad térmica of 0.17 - 0.19 W/(m·K) | ASTM D433 | |||||||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | UL 746B | |||||||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | UL 746B | |||||||
Temperatura de flexión bajo carga | 105 - 115 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 105 - 115 °C | ASTM D648 | 2 MPa | 248 °F/hr | |||||
112 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 112 °C | ISO 75-1/-2 | 2 MPa | dry | ||||||
125 - 140 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 125 - 140 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Temperatura de fusión | 165 - 172 °C Show Supplier Material materials with Temperatura de fusión of 165 - 172 °C | ASTM D3418 | |||||||
170 °C Show Supplier Material materials with Temperatura de fusión of 170 °C | ISO 11357-1/-3 | dry | 10°C/min | ||||||
Temperatura de transición del vidrio | -40.6 - -38.3 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40.6 - -38.3 °C | ASTM D7028 | |||||||
-40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | ISO 11357-1/-2 | dry | 10°C/min | ||||||
Thermal decomposition in air | 375 °C Show Supplier Material materials with Thermal decomposition in air of 375 °C | TGA | 1% wt. loss | ||||||
Thermal decomposition in nitrogen | 410 °C Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C | TGA | 1% wt. loss | ||||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Eléctrico
Property | Value | Frequency | Testing Standard | Condition |
---|---|---|---|---|
Constante dieléctrica | 4.5 - 9.5 [-] Show Supplier Material materials with Constante dieléctrica of 4.5 - 9.5 [-] | 1KHz | ASTM D150 | |
Factor de disipación | 0.01 - 0.21 [-] Show Supplier Material materials with Factor de disipación of 0.01 - 0.21 [-] | 100KHz | ASTM D150 | |
Rigidez dieléctrica | 63 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 63 kV/mm | ASTM D149 | ||
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | ASTM D257 | 65% RH |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de refracción | 1 [-] Show Supplier Material materials with Índice de refracción of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 2 % Show Supplier Material materials with Contracción of 2 % | dry | ISO 294-4 | |
2 % Show Supplier Material materials with Contracción of 2 % | dry | ISO 294-4 | Transverse | |
Melt viscosity | 200 - 500 Pa·s Show Supplier Material materials with Melt viscosity of 200 - 500 Pa·s | ASTM D3835 | ||
Thermal conductivity of melt | 0.19 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K) | |||
Velocidad de flujo de la masa derretida | 25 - 40 g/10min Show Supplier Material materials with Velocidad de flujo de la masa derretida of 25 - 40 g/10min | ASTM D1238 | 230°C/2.16kg | |
Velocidad de flujo del volumen derretido | 40 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 40 cm³/10min | dry | ISO 1133 | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Breathing Masks | |
Processing methods | Injection Molding: Compression Molding: |