General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 0.008 % Show Supplier Material materials with Absorción de agua of 0.008 % | Sim. to ISO 62 | |
Densidad | 1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry |
Índice límite de óxigeno | 42 % Show Supplier Material materials with Índice límite de óxigeno of 42 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 9 % Show Supplier Material materials with Elongation at yield of 9 % | dry | ISO 527-1/-2 | ||
Límite elástico | 50 MPa Show Supplier Material materials with Límite elástico of 50 MPa | dry | ISO 527-1/-2 | ||
Módulo elástico | 2 GPa Show Supplier Material materials with Módulo elástico of 2 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 36 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 36 kJ/m² | dry | ISO 179/1eA |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00015 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00015 1/K | dry | ISO 11359-1/-2 | ||||||
Temperatura de flexión bajo carga | 104 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 104 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Temperatura de fusión | 169 °C Show Supplier Material materials with Temperatura de fusión of 169 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-0 and yellow card available |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 2.5 % Show Supplier Material materials with Contracción of 2.5 % | dry | ISO 294-4 | |
2.5 % Show Supplier Material materials with Contracción of 2.5 % | dry | ISO 294-4 | Transverse | |
Thermal conductivity of melt | 0.19 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.19 W/(m·K) | |||
Velocidad de flujo del volumen derretido | 1.4 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 1.4 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Potable Water Distribution | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: |