General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.27 g/cm³ Show Supplier Material materials with Densidad of 1.27 g/cm³ | dry | ISO 1183 |
Mecánica
Aplicaciones térmicas
Property | Value | Testing Standard |
---|---|---|
Temperatura de fusión | 166 °C Show Supplier Material materials with Temperatura de fusión of 166 °C | ASTM D3418 |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt viscosity | 160 Pa·s Show Supplier Material materials with Melt viscosity of 160 Pa·s | ASTM D3835 | ||
Velocidad de flujo del volumen derretido | 12.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 12.5 cm³/10min | ISO 1133 | dry | 230°C/10kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines |