General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | Sim. to ISO 62 | |
Densidad | 1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.07 % Show Supplier Material materials with Moisture absorption of 0.07 % | Sim. to ISO 62 | |
Índice límite de óxigeno | 44 % Show Supplier Material materials with Índice límite de óxigeno of 44 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 | |
Límite elástico | 52 MPa Show Supplier Material materials with Límite elástico of 52 MPa | dry | ISO 527-1/-2 | |
Módulo elástico | 2.2 GPa Show Supplier Material materials with Módulo elástico of 2.2 GPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00015 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00015 1/K | dry | ISO 11359-1/-2 | ||||||
Temperatura de flexión bajo carga | 110 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 110 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
132 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 132 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||||||
Temperatura de fusión | 169 °C Show Supplier Material materials with Temperatura de fusión of 169 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Temperatura de reblandecimiento Vicat | 139 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 139 °C | ISO 306 | 50°C/h 50N | ||||||
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | dry | ISO 11357-1/-2 | 10°C/min | |||||
Inflamabilidad | At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard | Comment |
---|---|---|---|---|---|
Constante dieléctrica | 7 [-] Show Supplier Material materials with Constante dieléctrica of 7 [-] | dry | 1MHz | IEC 60250 | |
9 [-] Show Supplier Material materials with Constante dieléctrica of 9 [-] | dry | 100Hz | IEC 60250 | ||
Factor de disipación | 0.032 [-] Show Supplier Material materials with Factor de disipación of 0.032 [-] | dry | 100Hz | IEC 60250 | |
0.214 [-] Show Supplier Material materials with Factor de disipación of 0.214 [-] | dry | 1MHz | IEC 60250 | ||
Rigidez dieléctrica | 21 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 21 kV/mm | dry | IEC 60243-1 | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | cond. | IEC 60093 | min. | |
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | dry | IEC 60093 | ||
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 27 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 27 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Metal Tube Coating |