General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | dry | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 8 % Show Supplier Material materials with Elongation at yield of 8 % | dry | ISO 527-1/-2 | |
Límite elástico | 30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | dry | ISO 527-3 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Temperatura de flexión bajo carga | 108 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 108 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
Temperatura de fusión | 170 °C Show Supplier Material materials with Temperatura de fusión of 170 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Inflamabilidad | At thickness 0.8 mm IEC 60695-11-10: HB |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 15 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 15 cm³/10min | dry | ISO 1133 | 230°C/3.8kg |
Technological properties
Property | ||
---|---|---|
Application areas | Underground Fuel Containment |