General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 0.1 % Show Supplier Material materials with Absorción de agua of 0.1 % | Sim. to ISO 62 | |
Densidad | 1.77 g/cm³ Show Supplier Material materials with Densidad of 1.77 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.06 % Show Supplier Material materials with Moisture absorption of 0.06 % | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 46 % Show Supplier Material materials with Elongación of 46 % | dry | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
Límite elástico | 45 MPa Show Supplier Material materials with Límite elástico of 45 MPa | dry | ISO 527-3 | |
Módulo elástico | 1.5 GPa Show Supplier Material materials with Módulo elástico of 1.5 GPa | dry | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 157 °C Show Supplier Material materials with Temperatura de fusión of 157 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard |
---|---|---|---|---|
Constante dieléctrica | 6.5 [-] Show Supplier Material materials with Constante dieléctrica of 6.5 [-] | dry | 1MHz | IEC 60250 |
10.5 [-] Show Supplier Material materials with Constante dieléctrica of 10.5 [-] | dry | 100Hz | IEC 60250 | |
Factor de disipación | 0.038 [-] Show Supplier Material materials with Factor de disipación of 0.038 [-] | dry | 100Hz | IEC 60250 |
0.234 [-] Show Supplier Material materials with Factor de disipación of 0.234 [-] | dry | 1MHz | IEC 60250 | |
Rigidez dieléctrica | 21 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 21 kV/mm | dry | IEC 60243-1 | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | cond. | IEC 60093 | |
Volume resistivity | 2e+14 Ω·cm Show Supplier Material materials with Volume resistivity of 2e+14 Ω·cm | dry | IEC 60093 | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 25 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 25 cm³/10min | dry | ISO 1133 | 230°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Metal Tube Coating,Chemical Process Industry,Chemical Process Industry - Coating of Chemical Pumps,Chemical Process Industry - Coating of Chemical Valves,Chemical Process Industry - Coating of Chemical Vessels |