General
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 150 % Show Supplier Material materials with Elongación of 150 % | dry | ISO 527-3 | Transverse |
150 % Show Supplier Material materials with Elongación of 150 % | dry | ISO 527-3 | ||
Elongation at yield | 7 % Show Supplier Material materials with Elongation at yield of 7 % | dry | ISO 527-3 | |
Elongation at yield, transverse | 7 % Show Supplier Material materials with Elongation at yield, transverse of 7 % | dry | ISO 527-3 | |
Límite elástico | 29 MPa Show Supplier Material materials with Límite elástico of 29 MPa | dry | ISO 527-3 | |
30 MPa Show Supplier Material materials with Límite elástico of 30 MPa | dry | ISO 527-3 | Transverse | |
Resistencia a desgarros | 2 kN/m Show Supplier Material materials with Resistencia a desgarros of 2 kN/m | ISO 6383-1 | ||
3 kN/m Show Supplier Material materials with Resistencia a desgarros of 3 kN/m | ISO 6383-1 | Transverse | ||
Resistencia a la tracción | 30 MPa Show Supplier Material materials with Resistencia a la tracción of 30 MPa | dry | ISO 527-3 | Transverse |
30 MPa Show Supplier Material materials with Resistencia a la tracción of 30 MPa | dry | ISO 527-3 |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 100 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 100 kV/mm | dry | IEC 60243-1 |
Technological properties
Property | ||
---|---|---|
Application areas | Photovoltaic / Solar Film |