General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Densidad | 1.78 g/cm³ Show Supplier Material materials with Densidad of 1.78 g/cm³ | ASTM D792 | min. |
Aplicaciones térmicas
Property | Value | Testing Standard |
---|---|---|
Temperatura de fusión | 161 - 167 °C Show Supplier Material materials with Temperatura de fusión of 161 - 167 °C | ASTM D3418 |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 7000 - 7500 Pa·s Show Supplier Material materials with Melt viscosity of 7000 - 7500 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder |