General
Property | Value | Testing Standard |
---|---|---|
Densidad | 1.77 - 1.79 g/cm³ Show Supplier Material materials with Densidad of 1.77 - 1.79 g/cm³ | ASTM D792 |
Índice límite de óxigeno | 44 % Show Supplier Material materials with Índice límite de óxigeno of 44 % | ASTM D2863 |
Mecánica
Property | Temperature | Value | Testing Standard |
---|---|---|---|
Dureza Shore D | 76 - 80 [-] Show Supplier Material materials with Dureza Shore D of 76 - 80 [-] | ASTM D2240 | |
Elongación | 50 - 250 % Show Supplier Material materials with Elongación of 50 - 250 % | ASTM D638 | |
Impact strength, Charpy notched, ASTM | 23 °C | 107 - 320 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 107 - 320 J/m | ASTM D256 |
Límite elástico | 40 - 55.2 MPa Show Supplier Material materials with Límite elástico of 40 - 55.2 MPa | ASTM D638 | |
Módulo de flexión | 1.4 - 2.2 GPa Show Supplier Material materials with Módulo de flexión of 1.4 - 2.2 GPa | ASTM D790 | |
Resistencia a la compresión | 68.9 - 103 MPa Show Supplier Material materials with Resistencia a la compresión of 68.9 - 103 MPa | ASTM D695 | |
Resistencia a la tracción | 34 - 43 MPa Show Supplier Material materials with Resistencia a la tracción of 34 - 43 MPa | ASTM D638 |
Aplicaciones térmicas
Property | Value | Testing Standard |
---|---|---|
Temperatura de fusión | 165 - 342 °C Show Supplier Material materials with Temperatura de fusión of 165 - 342 °C | ASTM D3418 |
Óptico
Property | Value | Testing Standard | Comment |
---|---|---|---|
Índice de refracción | 1 [-] Show Supplier Material materials with Índice de refracción of 1 [-] | ASTM D542 | sodium D line |
Rheological Properties
Property | Value | Testing Standard |
---|---|---|
Melt viscosity | 7000 - 7500 Pa·s Show Supplier Material materials with Melt viscosity of 7000 - 7500 Pa·s | ASTM D3835 |
Technological properties
Property | ||
---|---|---|
Application areas | Lithium Ion Battery Binder |