General
Property | Value | Testing Standard |
---|---|---|
Absorción de agua | 0 % Show Supplier Material materials with Absorción de agua of 0 % | Sim. to ISO 62 |
Densidad | 1.87 - 1.89 g/cm³ Show Supplier Material materials with Densidad of 1.87 - 1.89 g/cm³ | ASTM D792 |
Moisture absorption | 0 % Show Supplier Material materials with Moisture absorption of 0 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elongación | 3 % Show Supplier Material materials with Elongación of 3 % | dry | ASTM D638, ISO 527-1/-2 | min. | |
Impact strength, Charpy notched, ASTM | 23 °C | 101 J/m Show Supplier Material materials with Impact strength, Charpy notched, ASTM of 101 J/m | ASTM D256 | ||
Límite elástico | 120 MPa Show Supplier Material materials with Límite elástico of 120 MPa | ASTM D638 | |||
Módulo de flexión | 6.6 GPa Show Supplier Material materials with Módulo de flexión of 6.6 GPa | ASTM D790 | |||
Módulo elástico | 0.788 GPa Show Supplier Material materials with Módulo elástico of 0.788 GPa | ASTM D638 | |||
7.9 GPa Show Supplier Material materials with Módulo elástico of 7.9 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la flexión | 174 MPa Show Supplier Material materials with Resistencia a la flexión of 174 MPa | ASTM D790 | at 5% strain | ||
Resistencia a la tracción | 120 MPa Show Supplier Material materials with Resistencia a la tracción of 120 MPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy no entallado | 23 °C | 44 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy no entallado of 44 kJ/m² | dry | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 3.5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-05 1/K | dry | ISO 11359-1/-2 | Transverse | |||||
3.5e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 3.5e-05 1/K | dry | ISO 11359-1/-2 | |||||||
Temperatura de flexión bajo carga | 159 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 159 °C | dry | ASTM D648, ISO 75-1/-2 | 2 MPa | 248 °F/hr | ||||
160 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 160 °C | ASTM D648 | 0.45 MPa | 248 °F/hr | ||||||
Temperatura de fusión | 165 - 172 °C Show Supplier Material materials with Temperatura de fusión of 165 - 172 °C | ASTM D3418 | |||||||
170 °C Show Supplier Material materials with Temperatura de fusión of 170 °C | dry | ISO 11357-1/-3 | 10°C/min | ||||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: V-0 |
Rheological Properties
Property | Value | Condition | Testing Standard |
---|---|---|---|
Contracción | 0.25 - 1 % Show Supplier Material materials with Contracción of 0.25 - 1 % | 50% RH | ASTM D955 |
Technological properties
Property | ||
---|---|---|
Application areas | Fittings, Components, and Injection Molded Parts,Chemical Process Industry,Chemical Process Industry - Injection Molding,Chemical Process Industry - Stock Shapes,Tower Packing | |
Fillers | Glass Fiber | |
Processing methods | Injection Molding: |