General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. |
Límite elástico | 28 MPa Show Supplier Material materials with Límite elástico of 28 MPa | dry | ISO 527-1/-2 | |
Módulo elástico | 0.572 GPa Show Supplier Material materials with Módulo elástico of 0.572 GPa | cond. | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 215 °C Show Supplier Material materials with Temperatura de fusión of 215 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 1 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 1 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Conditioning Circuit | |
Processing methods | Extrusion: |