General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 55 [-] Show Supplier Material materials with Dureza Shore D of 55 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | |
Límite elástico | 24 MPa Show Supplier Material materials with Límite elástico of 24 MPa | cond. | ISO 527-1/-2 | ||
35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | dry | ISO 527-3 | |||
49 MPa Show Supplier Material materials with Límite elástico of 49 MPa | dry | ISO 527-2/-2 | |||
Módulo elástico | 0.5 GPa Show Supplier Material materials with Módulo elástico of 0.5 GPa | cond. | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 21.6 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 21.6 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 83 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 83 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 75 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 75 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 1.1 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 1.1 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Alternative Fuel Systems - CNG, LPG, LNG Lines and Tanks | |
Processing methods | Blow Molding: |