General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 5.5 % Show Supplier Material materials with Absorción de agua of 5.5 % | Sim. to ISO 62 | |
Densidad | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 57 [-] Show Supplier Material materials with Dureza Shore D of 57 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal, nominal | |
Elongation at yield | 22 % Show Supplier Material materials with Elongation at yield of 22 % | dry | ISO 527-1/-2 | ||
28 % Show Supplier Material materials with Elongation at yield of 28 % | cond. | ISO 527-1/-2 | |||
Límite elástico | 25 MPa Show Supplier Material materials with Límite elástico of 25 MPa | dry | ISO 527-3 | ||
42 MPa Show Supplier Material materials with Límite elástico of 42 MPa | cond. | ISO 527-1/-2 | |||
44 MPa Show Supplier Material materials with Límite elástico of 44 MPa | dry | ISO 527-2/-2 | |||
Módulo elástico | 0.65 GPa Show Supplier Material materials with Módulo elástico of 0.65 GPa | cond. | ISO 527-1/-2 | ||
0.85 GPa Show Supplier Material materials with Módulo elástico of 0.85 GPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 82 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 82 kJ/m² | dry | ISO 179/1eA | |
23 °C | 89 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 89 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.0002 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.0002 1/K | dry | ISO 11359-1/-2 | ||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Temperatura de reblandecimiento Vicat | 86 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 86 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At Thickness 3.2 mm IEC 60695-11-10: HB |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 3.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 3.5 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Tubing and Hoses,Offshore Flexible Pipes | |
Processing methods | Injection Molding: Extrusion: |