General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 6 % Show Supplier Material materials with Absorción de agua of 6 % | Sim. to ISO 62 | |
Densidad | 1.05 g/cm³ Show Supplier Material materials with Densidad of 1.05 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 67 [-] Show Supplier Material materials with Dureza Shore D of 67 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
550 % Show Supplier Material materials with Elongación of 550 % | dry | ISO 527-3 | Transverse | ||
610 % Show Supplier Material materials with Elongación of 610 % | dry | ISO 527-3 | |||
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-2/-2 | ||
6 % Show Supplier Material materials with Elongation at yield of 6 % | cond. | ISO 527-1/-2 | |||
16 % Show Supplier Material materials with Elongation at yield of 16 % | dry | ISO 527-3 | |||
Elongation at yield, transverse | 16 % Show Supplier Material materials with Elongation at yield, transverse of 16 % | dry | ISO 527-3 | ||
Límite elástico | 35 MPa Show Supplier Material materials with Límite elástico of 35 MPa | dry | ISO 527-3 | Transverse | |
36 MPa Show Supplier Material materials with Límite elástico of 36 MPa | cond. | ISO 527-1/-2 | |||
Módulo elástico | 1.8 GPa Show Supplier Material materials with Módulo elástico of 1.8 GPa | cond. | ISO 527-1/-2 | ||
2 GPa Show Supplier Material materials with Módulo elástico of 2 GPa | dry | ISO 527-1/-2 | |||
Resistencia a la tracción | 55 MPa Show Supplier Material materials with Resistencia a la tracción of 55 MPa | dry | ISO 527-3 | Transverse | |
61 MPa Show Supplier Material materials with Resistencia a la tracción of 61 MPa | dry | ISO 527-3 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 23 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 23 kJ/m² | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | cond. | ISO 179/1eU | ||
Tear force | 45 N Show Supplier Material materials with Tear force of 45 N | ISO 6383-2 | |||
55 N Show Supplier Material materials with Tear force of 55 N | ISO 6383-2 | Transverse |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Temperatura de flexión bajo carga | 50 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 50 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
80 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 80 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Temperatura de reblandecimiento Vicat | 128 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 128 °C | ISO 306 | 50°C/h 50N | ||||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 4 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 4 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fuel Management - Fuel Lines,Conveyor Belts and Pulleys,Underground Fuel Containment | |
Certifications | European Food Contact | |
Processing methods | Injection Molding: Extrusion: |