General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 5 % Show Supplier Material materials with Absorción de agua of 5 % | Sim. to ISO 62 | |
Densidad | 1.04 g/cm³ Show Supplier Material materials with Densidad of 1.04 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.1 % Show Supplier Material materials with Moisture absorption of 1.1 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 50 [-] Show Supplier Material materials with Dureza Shore D of 50 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | |
Módulo elástico | 0.3 GPa Show Supplier Material materials with Módulo elástico of 0.3 GPa | cond. | ISO 527-1/-2 | ||
0.6 GPa Show Supplier Material materials with Módulo elástico of 0.6 GPa | dry | ISO 527-1/-2 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 80 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 80 kJ/m² | dry | ISO 179/1eA | |
23 °C | 84 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 84 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Temperatura de flexión bajo carga | 60 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 60 °C | dry | ISO 75-1/-2 | 0.45 MPa | |||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Temperatura de reblandecimiento Vicat | 62 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 62 °C | ISO 306 | 50°C/h 50N | ||||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 0.7 % Show Supplier Material materials with Contracción of 0.7 % | dry | ISO 294-4 | |
0.9 % Show Supplier Material materials with Contracción of 0.9 % | dry | ISO 294-4 | Transverse | |
Velocidad de flujo del volumen derretido | 2.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2.5 cm³/10min | dry | ISO 1133 | 235°C/5kg |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Conditioning Circuit | |
Processing methods | Injection Molding: Extrusion: |