General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 3.3 % Show Supplier Material materials with Absorción de agua of 3.3 % | Sim. to ISO 62 | |
Densidad | 1.03 g/cm³ Show Supplier Material materials with Densidad of 1.03 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.3 % Show Supplier Material materials with Moisture absorption of 1.3 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 73 [-] Show Supplier Material materials with Dureza Shore D of 73 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal | |
530 % Show Supplier Material materials with Elongación of 530 % | dry | ISO 527-3 | Transverse | ||
530 % Show Supplier Material materials with Elongación of 530 % | dry | ISO 527-3 | |||
Elongation at yield | 3.4 % Show Supplier Material materials with Elongation at yield of 3.4 % | cond. | ISO 527-1/-2 | ||
20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-3 | |||
Elongation at yield, transverse | 15 % Show Supplier Material materials with Elongation at yield, transverse of 15 % | dry | ISO 527-3 | ||
Límite elástico | 33 MPa Show Supplier Material materials with Límite elástico of 33 MPa | dry | ISO 527-3 | Transverse | |
47 MPa Show Supplier Material materials with Límite elástico of 47 MPa | cond. | ISO 527-1/-2 | |||
55 MPa Show Supplier Material materials with Límite elástico of 55 MPa | dry | ISO 527-1/-2 | |||
Módulo elástico | 1.9 GPa Show Supplier Material materials with Módulo elástico of 1.9 GPa | cond. | ISO 527-1/-2 | ||
Resistencia a la tracción | 60 MPa Show Supplier Material materials with Resistencia a la tracción of 60 MPa | dry | ISO 527-3 | Transverse | |
80 MPa Show Supplier Material materials with Resistencia a la tracción of 80 MPa | dry | ISO 527-3 | |||
Resistencia al choque, ensayo Charpy entallado | 23 °C | 9 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 9 kJ/m² | cond. | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23°C | cond. | ISO 179/1eU | ||
Tear force | 35 N Show Supplier Material materials with Tear force of 35 N | ISO 6383-2 | Transverse | ||
40 N Show Supplier Material materials with Tear force of 40 N | ISO 6383-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Pressure | Comment | ||||
---|---|---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 9.3e-05 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 9.3e-05 1/K | dry | ISO 11359-1/-2 | ||||||
0.000133 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.000133 1/K | dry | ISO 11359-1/-2 | Transverse | ||||||
Temperatura de flexión bajo carga | 75 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 75 °C | dry | ISO 75-1/-2 | 2 MPa | |||||
130 °C Show Supplier Material materials with Temperatura de flexión bajo carga of 130 °C | dry | ISO 75-1/-2 | 0.45 MPa | ||||||
Temperatura de fusión | 220 °C Show Supplier Material materials with Temperatura de fusión of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |||||
Temperatura de reblandecimiento Vicat | 134 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 134 °C | ISO 306 | 50°C/h 50N | ||||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At thickness 3.2 mm IEC 60695-11-10: HB |
Eléctrico
Property | Value | Condition | Frequency | Testing Standard | Comment |
---|---|---|---|---|---|
Constante dieléctrica | 3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | cond. | 100Hz | IEC 60250 | |
3 [-] Show Supplier Material materials with Constante dieléctrica of 3 [-] | IEC 60250 | 1MHz | |||
Factor de disipación | 0.025 [-] Show Supplier Material materials with Factor de disipación of 0.025 [-] | cond. | 1MHz | IEC 60250 | |
0.062 [-] Show Supplier Material materials with Factor de disipación of 0.062 [-] | cond. | 100Hz | IEC 60250 | ||
Rigidez dieléctrica | 38 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 38 kV/mm | cond., dry | IEC 60243-1 | ||
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | cond. | IEC 60093 | min. | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | cond. | IEC 60093 | min. | |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Velocidad de flujo del volumen derretido | 2.5 cm³/10min Show Supplier Material materials with Velocidad de flujo del volumen derretido of 2.5 cm³/10min | dry | ISO 1133 | 235°C/2.16kg |
Technological properties
Property | ||
---|---|---|
Application areas | Mold Release Film | |
Processing methods | Injection Molding: Film Extrusion: |