General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Densidad | 1.12 g/cm³ Show Supplier Material materials with Densidad of 1.12 g/cm³ | dry | ISO 1183 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 4.4 % Show Supplier Material materials with Elongation at yield of 4.4 % | cond. | ISO 527-1/-2 | |
Límite elástico | 48 MPa Show Supplier Material materials with Límite elástico of 48 MPa | cond. | ISO 527-1/-2 | |
80 MPa Show Supplier Material materials with Límite elástico of 80 MPa | dry | ISO 527-1/-2 | ||
Módulo elástico | 2.3 GPa Show Supplier Material materials with Módulo elástico of 2.3 GPa | cond. | ISO 527-1/-2 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 229 °C Show Supplier Material materials with Temperatura de fusión of 229 °C | dry | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Application areas | Fluid Management - Air Conditioning Circuit | |
Processing methods | Extrusion: |