General
Property | Value | Testing Standard | Comment |
---|---|---|---|
Coarse particles amount | 10 % Show Supplier Material materials with Coarse particles amount of 10 % | ISO 13319 | max. |
Coarse particles size | 40 μm Show Supplier Material materials with Coarse particles size of 40 μm | min. | |
Densidad | 0.375 g/cm³ Show Supplier Material materials with Densidad of 0.375 g/cm³ | ISO 1068 | apparent density unpacked |
Fine particles amount | 5 % Show Supplier Material materials with Fine particles amount of 5 % | ISO 13319 | max. |
Fine particles size | 20 μm Show Supplier Material materials with Fine particles size of 20 μm | max. | |
Median particles size | 30 μm Show Supplier Material materials with Median particles size of 30 μm | ISO 13319 | |
Área superficial específica | 1 m²/g Show Supplier Material materials with Área superficial específica of 1 m²/g | ISO 9277 |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard |
---|---|---|---|
Temperatura de fusión | 177 °C Show Supplier Material materials with Temperatura de fusión of 177 °C | dry | ISO 11357-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Coating Additives,Coating Additives - Coil Coating,Coating Additives - Floor Coating,Coating Additives - Wood Coating |