General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.2 % Show Supplier Material materials with Absorción de agua of 1.2 % | Sim. to ISO 62 | |
Densidad | 1 g/cm³ Show Supplier Material materials with Densidad of 1 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 |
Mecánica
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Dureza Shore A | 90 [-] Show Supplier Material materials with Dureza Shore A of 90 [-] | ISO 7619-1 | for 3 seconds | |
Dureza Shore D | 35 [-] Show Supplier Material materials with Dureza Shore D of 35 [-] | ISO 7619-1 | dry | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | ISO 527-1/-2 | cond., dry | min. |
Módulo elástico | 0.071 GPa Show Supplier Material materials with Módulo elástico of 0.071 GPa | ISO 527-1/-2 | cond. | |
0.073 GPa Show Supplier Material materials with Módulo elástico of 0.073 GPa | ISO 527-1/-2 | dry | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23 and -30°C | ISO 179/1eA | cond. | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | ISO 179/1eU | cond. |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 160 °C Show Supplier Material materials with Temperatura de fusión of 160 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 131 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 131 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | USP Class VI | |
Processing methods | Injection Molding: Extrusion: |