General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.2 % Show Supplier Material materials with Absorción de agua of 1.2 % | Sim. to ISO 62 | |
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.6 % Show Supplier Material materials with Moisture absorption of 0.6 % | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 50 [-] Show Supplier Material materials with Dureza Shore D of 50 [-] | dry | ISO 7619-1 | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal |
Elongation at yield | 25 % Show Supplier Material materials with Elongation at yield of 25 % | cond., dry | ISO 527-1/-2 | |
Límite elástico | 12 MPa Show Supplier Material materials with Límite elástico of 12 MPa | dry | ISO 527-1/-2 | |
17 MPa Show Supplier Material materials with Límite elástico of 17 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.165 GPa Show Supplier Material materials with Módulo elástico of 0.165 GPa | cond. | ISO 527-1/-2 | |
0.17 GPa Show Supplier Material materials with Módulo elástico of 0.17 GPa | dry | ISO 527-1/-2 | ||
Resistencia al choque, ensayo Charpy entallado | No Break at 23 and -30°C | cond. | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 159 °C Show Supplier Material materials with Temperatura de fusión of 159 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 142 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 142 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Healthcare-Other,IV Bags,Medical Catheters | |
Certifications | USP Class VI | |
Processing methods | Injection Molding: Extrusion: |