General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.1 % Show Supplier Material materials with Absorción de agua of 1.1 % | Sim. to ISO 62 | |
Densidad | 1.01 g/cm³ Show Supplier Material materials with Densidad of 1.01 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.7 % Show Supplier Material materials with Moisture absorption of 0.7 % | Sim. to ISO 62 |
Mecánica
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dureza Shore D | 61 [-] Show Supplier Material materials with Dureza Shore D of 61 [-] | dry | ISO 7619-1 | 15 seconds | |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. | nominal | |
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | cond. | ISO 527-1/-2 | ||
22 % Show Supplier Material materials with Elongation at yield of 22 % | dry | ISO 527-1/-2 | |||
Límite elástico | 26 MPa Show Supplier Material materials with Límite elástico of 26 MPa | cond. | ISO 527-1/-2 | ||
Módulo elástico | 0.39 GPa Show Supplier Material materials with Módulo elástico of 0.39 GPa | cond. | ISO 527-1/-2 | ||
0.414 GPa Show Supplier Material materials with Módulo elástico of 0.414 GPa | dry | ISO 527-1/-2 | |||
Resistencia a desgarros | 149 kN/m Show Supplier Material materials with Resistencia a desgarros of 149 kN/m | ISO 34-1 | |||
Resistencia al choque, ensayo Charpy entallado | -30 °C | 20 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 20 kJ/m² | cond. | ISO 179/1eA | |
23 °C | 120 kJ/m² Show Supplier Material materials with Resistencia al choque, ensayo Charpy entallado of 120 kJ/m² | cond. | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Coeficiente de dilatación térmica | 0.00016 1/K Show Supplier Material materials with Coeficiente de dilatación térmica of 0.00016 1/K | dry | ISO 11359-1/-2 | ||||
Temperatura de fusión | 172 °C Show Supplier Material materials with Temperatura de fusión of 172 °C | dry | ISO 11357-1/-3 | 10°C/min | |||
Temperatura de reblandecimiento Vicat | 164 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 164 °C | ISO 306 | 50°C/h 50N | ||||
Inflamabilidad | At thickness 1.6 mm IEC 60695-11-10: HB, At Thickness 3.1 mm IEC 60695-11-10: HB and yellow card available |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 4e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 4e+13 Ω/sq | cond. | IEC 60093 |
Índice de seguimiento comparativo | 600 V Show Supplier Material materials with Índice de seguimiento comparativo of 600 V | cond. | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Contracción | 1.2 % Show Supplier Material materials with Contracción of 1.2 % | dry | ISO 294-4 | |
1.5 % Show Supplier Material materials with Contracción of 1.5 % | dry | ISO 294-4 | Transverse | |
Density of melt | 0.83 g/cm³ Show Supplier Material materials with Density of melt of 0.83 g/cm³ | |||
Specific heat capacity melt | 2700 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2700 J/(kg·K) | |||
Thermal conductivity of melt | 0.2 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.2 W/(m·K) |
Technological properties
Property | ||
---|---|---|
Application areas | Textile - Others,Footwear - Outsoles,Ski Boots,Sports Equipment | |
Certifications | Yellow Card | |
Processing methods | Injection Molding: Extrusion: |