General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 120 % Show Supplier Material materials with Absorción de agua of 120 % | Sim. to ISO 62 | |
Densidad | 1.14 g/cm³ Show Supplier Material materials with Densidad of 1.14 g/cm³ | ISO 1183 | dry |
Moisture absorption | 4.5 % Show Supplier Material materials with Moisture absorption of 4.5 % | Sim. to ISO 62 |
Mecánica
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 200 °C Show Supplier Material materials with Temperatura de fusión of 200 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+07 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+07 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 100000 Ω·cm Show Supplier Material materials with Volume resistivity of 100000 Ω·cm | cond. | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Permanent Antistatic Solutions,Permanent Antistatic Solutions E&E | |
Processing methods | Injection Molding: Extrusion: |