General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 48 % Show Supplier Material materials with Absorción de agua of 48 % | Sim. to ISO 62 | |
Densidad | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | Sim. to ISO 62 | |
Índice límite de óxigeno | 19 % Show Supplier Material materials with Índice límite de óxigeno of 19 % | ISO 4589-1/-2 | dry |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 40 [-] Show Supplier Material materials with Dureza Shore D of 40 [-] | dry | ISO 7619-1 | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond., dry | ISO 527-1/-2 | min. |
500 % Show Supplier Material materials with Elongación of 500 % | dry | ISO 527-3 | ||
700 % Show Supplier Material materials with Elongación of 700 % | dry | ISO 527-3 | Transverse | |
Módulo elástico | 0.08 GPa Show Supplier Material materials with Módulo elástico of 0.08 GPa | cond. | ISO 527-1/-2 | |
0.097 GPa Show Supplier Material materials with Módulo elástico of 0.097 GPa | dry | ISO 527-1/-2 | ||
Resistencia a la tracción | 32 MPa Show Supplier Material materials with Resistencia a la tracción of 32 MPa | dry | ISO 527-3 | |
34 MPa Show Supplier Material materials with Resistencia a la tracción of 34 MPa | dry | ISO 527-3 | Transverse | |
Resistencia al choque, ensayo Charpy entallado | No Break at 23°C | cond. | ISO 179/1eA | |
No Break at 23 and -30°C | dry | ISO 179/1eA | ||
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 158 °C Show Supplier Material materials with Temperatura de fusión of 158 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de transición del vidrio | -40 °C Show Supplier Material materials with Temperatura de transición del vidrio of -40 °C | dry | ISO 11357-1/-2 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Rigidez dieléctrica | 5 kV/mm Show Supplier Material materials with Rigidez dieléctrica of 5 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 3e+09 Ω/sq Show Supplier Material materials with Surface resistivity of 3e+09 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 2.5e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 2.5e+07 Ω·cm | cond. | IEC 60093 |
1.5e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1.5e+11 Ω·cm | dry | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Permanent Antistatic Solutions,Footwear - Midsoles / Foam,Permanent Antistatic Solutions E&E | |
Processing methods | Injection Molding: Extrusion: |