General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 48 % Show Supplier Material materials with Absorción de agua of 48 % | Sim. to ISO 62 | |
Densidad | 1.07 g/cm³ Show Supplier Material materials with Densidad of 1.07 g/cm³ | ISO 1183 | dry |
Moisture absorption | 1.4 % Show Supplier Material materials with Moisture absorption of 1.4 % | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 40 [-] Show Supplier Material materials with Dureza Shore D of 40 [-] | dry | ISO 7619-1 | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. |
Módulo elástico | 0.08 GPa Show Supplier Material materials with Módulo elástico of 0.08 GPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 160 °C Show Supplier Material materials with Temperatura de fusión of 160 °C | dry | ISO 11357-1/-3 | 10°C/min |
Eléctrico
Property | Value | Condition | Testing Standard |
---|---|---|---|
Surface resistivity | 1e+07 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+07 Ω/sq | cond. | IEC 60093 |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | cond. | IEC 60093 |
Technological properties
Property | ||
---|---|---|
Application areas | Permanent Antistatic Solutions,Permanent Antistatic Solutions E&E | |
Processing methods | Injection Molding: Extrusion: |