General
Property | Value | Testing Standard | Condition |
---|---|---|---|
Absorción de agua | 1.3 % Show Supplier Material materials with Absorción de agua of 1.3 % | Sim. to ISO 62 | |
Bio-based content | 28 % Show Supplier Material materials with Bio-based content of 28 % | ||
32 % Show Supplier Material materials with Bio-based content of 32 % | |||
Densidad | 1.02 g/cm³ Show Supplier Material materials with Densidad of 1.02 g/cm³ | ISO 1183 | dry |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | Sim. to ISO 62 |
Mecánica
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dureza Shore D | 25 [-] Show Supplier Material materials with Dureza Shore D of 25 [-] | dry | ISO 7619-1 | 15 seconds |
Elongación | 50 % Show Supplier Material materials with Elongación of 50 % | cond. | ISO 527-1/-2 | min. |
Módulo elástico | 0.04 GPa Show Supplier Material materials with Módulo elástico of 0.04 GPa | cond. | ISO 527-1/-2 | |
Resistencia al choque, ensayo Charpy entallado | No Break at 23 and -30°C | cond., dry | ISO 179/1eA | |
Resistencia al choque, ensayo Charpy no entallado | No Break at 23 and -30°C | dry and cond. | ISO 179/1eU |
Aplicaciones térmicas
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Temperatura de fusión | 135 °C Show Supplier Material materials with Temperatura de fusión of 135 °C | dry | ISO 11357-1/-3 | 10°C/min |
Temperatura de reblandecimiento Vicat | 81 °C Show Supplier Material materials with Temperatura de reblandecimiento Vicat of 81 °C | ISO 306 | 50°C/h 50N |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Breathable Films - Housewrap,Permanent Antistatic Solutions,Eyewear Frames,Footwear - Midsoles / Foam | |
Processing methods | Injection Molding: Extrusion: |